MDT-file: Download

Test structure on the base of SiO2 stripes height 0.1µm grating on the silicon wafer. Ion implantation by boron with E=100 keV, annealing and  SiO2 layer etching was employed. On the resulting structure following images were obtained: Fig. 1 - Topography of test structure (contact mode AFM), Fig. 2. - Profile of test structure, Fig. 3. - Contact SCM image of the same area, Fig. 4. - Profile of Contact SCM image.


a
a
Test structure

Test structure on the base of SiO2 stripes height 0.1µm grating on the silicon wafer. Ion implantation by boron with E=100 keV, annealing and  SiO2 layer etching was employed. On the resulting structure following images were obtained: Fig. 1 - Topography of test structure (contact mode AFM), Fig. 2. - Profile of test structure, Fig. 3. - Contact SCM image of the same area, Fig. 4. - Profile of Contact SCM image.


size: 18x28 um