+86 21 6079 0303
+86 135 2487 5604

Erythrite

MDT-file: Download

Surface of an eritrite deposit solution on pyroceram substrate.
The eritrite solution after electrolysis was processed by ultrasound during 5 hours. Then deposit was carried out from a bottom of a test tube on a pyroceram surface after end of ultrasound process.

Image courtesy of Gusev E. Yu., Taganrog State University Of Radioengineering.
The sample was kindly given by Kuzharov A.A., Sokolenko A.I, Don State Technical University.


erythrite3d
erythrite3d
Erythrite

Surface of an eritrite deposit solution on pyroceram substrate.
The eritrite solution after electrolysis was processed by ultrasound during 5 hours. Then deposit was carried out from a bottom of a test tube on a pyroceram surface after end of ultrasound process.

Image courtesy of Gusev E. Yu., Taganrog State University Of Radioengineering.
The sample was kindly given by Kuzharov A.A., Sokolenko A.I, Don State Technical University.


size: 10x10 um
SPM principle: Intermittent contact mode
Have more questions? Contact us +7-499-110-2050
or fulfill a form and we will answer all your questions.